Friction Stir Welding: How It Works Step by Step

Friction stir welding joins aluminum and other metals without melting them. A rotating tool presses into the joint line, generates heat through friction and plastic deformation, and moves along the seam while the material flows around the pin and consolidates behind the shoulder. The sequence looks simple from the outside, but the result depends on tool geometry, clamping, backing support, and controlled machine motion. This guide walks through the process step by step, shows what happens at each stage, and explains which visual checks are useful and which conclusions a photograph cannot support.

Why Friction Stir Welding Stays in the Solid State

Friction stir welding is a solid-state joining process. A non-consumable tool with a shoulder and a pin rotates, plunges into the joint line, and moves along the seam. The workpiece is not melted. Heat comes from friction between the tool and the workpiece and from plastic deformation of the material. The softened material flows around the pin and is consolidated by the shoulder as the tool passes.

That description is accurate but incomplete. The tool does three jobs at once: it generates heat, it transports material from the leading edge to the trailing edge, and it forges the plasticized zone behind the pin. If any one of those jobs is weak, the weld can look acceptable on the surface and still contain a tunnel, void, or incomplete root consolidation. The process is therefore controlled by the combination of tool geometry, machine stiffness, fixture rigidity, and parameter settings, not by rotation speed alone.

Because the material stays solid, FSW avoids the solidification defects that affect fusion welding of aluminum, such as gas porosity and hot cracking. It does not remove every defect risk. The defects that matter in FSW are flow related: lack of fill, tunnel defects, voids, flash, and incomplete penetration. Each one has a process cause that can be checked.

The FSW Process Step by Step

The sequence below describes a conventional linear FSW pass. The same logic applies to curved seams and spot variants, but the tool path and retraction method change.

  1. Prepare the joint and fixture. Clean the faying surfaces, control the gap and mismatch, and clamp both plates to a backing plate. The fixture must hold the plates flat and prevent lifting as the tool pushes down. Check clamp pressure, backing plate flatness, and groove alignment before the first pass.

  2. Position the tool and set the plunge depth. The tool axis is tilted slightly relative to the workpiece, and the shoulder must contact the surface at the intended depth. The tilt and plunge depth are part of the procedure, not operator preference. A shallow shoulder contact may fail to contain the plasticized material; excessive plunge can thin the joint and overload the machine.

  3. Plunge and dwell. The tool rotates and enters the joint. The pin displaces material, the shoulder heats and contains it, and the axial force rises. The dwell continues until the force and torque signals stabilize. A short or inconsistent dwell can leave the start zone underheated; an excessive dwell can overheat the start and create flash.

  4. Traverse along the seam. The machine moves the tool along the joint while maintaining rotation speed, travel speed, and axial force. Material passes from the leading edge around the pin and consolidates behind the shoulder. The operator or controller watches force, torque, spindle speed, and seam position. Any drift in these signals is a reason to stop and check the setup, not to finish the pass and inspect later.

  5. Finish the pass and manage the exit. A conventional tool leaves a keyhole where the pin withdraws. A retractable tool withdraws the pin into the shoulder and lets plasticized material fill the hole. A runoff tab can also move the keyhole outside the part. The choice depends on whether the joint is closed, whether the hole is acceptable, and whether post-processing can remove it.

  6. Release and inspect. Let the weld cool under the fixture, release the clamps, and inspect the surface, flash, edge condition, and start and stop zones. Record the parameter trace and mark the weld for traceability. A visual pass is an initial screen, not a release decision.

What the Tool Does at Each Stage

The tool is the most direct control over material flow. The shoulder diameter sets the heated zone and the forging footprint. A larger shoulder adds heat and containment but also raises torque and flash risk. The pin length sets penetration; too short and the root may not consolidate, too long and the pin can contact the backing plate. Pin profile, whether threaded, tapered, or fluted, changes how material moves downward and around the tool.

Conventional FSW tool

Tool material must survive the working temperature and abrasion of the alloy being welded. Tool steel is common for many aluminum alloys; tungsten carbide and PCBN are used where the workpiece is harder or the tool temperature is higher. The choice is not a grade label to copy from a catalog. It follows the alloy, thickness, joint type, and production volume, and it must be matched to the spindle and holder that will carry it.

The spindle and tool holder are part of the process. A stiff spindle with low runout holds the tool on the intended axis and transmits torque without vibration. The holder interface must match the tool shank and the machine taper. If the tool is changed between passes, the clamping repeatability matters as much as the tool geometry. A tool that sits slightly off-center or not fully seated can produce an asymmetric weld or a force spike at the start.

Friction Stir Welding Spindle Series

Tool geometry is only part of the setup; the spindle interface and optional tool features determine how repeatably the tool can be changed and controlled. <AEE provides customer with optional features FSW tool> covers optional features for FSW tools.

How Rotation, Travel, Force and Tilt Change the Weld

Rotation speed, travel speed, axial force, and tilt angle interact. Changing one changes the others. Rotation speed controls heat generation and the stirring action. Travel speed controls how much heat is delivered per unit length and how fast the tool moves through the plasticized zone. Axial force controls shoulder contact and forging pressure. Tilt angle helps the shoulder pack material behind the pin and controls flash.

ParameterWhat it controlsRisk when too lowRisk when too highFirst check
Rotation speedHeat generation and stirring actionCold material, poor flow, tunnel riskExcess flash, softened zone, tool wearCompare force and torque with a known-good coupon
Travel speedHeat input per unit length and cycle timeOverheating, wide flash, distortionLack of fill, tunnel risk, high tool loadCheck seam fill and run a coupon at the next speed
Axial forceShoulder contact and forging pressureIncomplete consolidation, weak rootThinning, flash, backing plate loadReview force trace and backing plate condition
Tilt angleShoulder packing and material containmentMaterial escapes, poor consolidationShoulder digs, surface markingInspect shoulder mark and flash pattern

The table is a starting point for diagnosis, not a recipe. The same parameter change can produce different results on a thin sheet and a thick plate, or on a heat-treatable alloy and a solid-solution alloy. A 6xxx alloy that responds well to one tool may soften excessively in the heat-affected zone with a hotter parameter set. A copper joint may need a different tool material and a narrower window because the heat drains faster and the tool load is higher.

Force control and position control are different strategies. Position control holds the plunge depth and lets axial force vary with thermal conditions. Force control holds axial force and lets depth vary. Position control can be simpler for a stable process; force control can protect the tool and the backing plate when the workpiece is less consistent. The machine structure must be stiff enough for the chosen strategy. A flexible fixture or a worn backing plate can make a good parameter set behave poorly.

Dissimilar joints narrow the window further. The tool must stir both materials without excessive intermetallic growth or tool overload. Offsetting the pin toward the softer or lower-melting alloy, controlling the interface position, and limiting the heat input are common process levers. These are procedure decisions, not adjustments to make after the first weld looks poor.

When the joint pairs different alloys, the parameter window narrows and the tool offset becomes part of the process definition. <Customized Dissimilar Material Welding Manufacturers in China> covers customized dissimilar-material welding requirements.

What the Weld Zone Looks Like in a Cross Section

A cross section through an FSW joint usually shows four regions. The nugget, or stir zone, is the central region that the pin has deformed and recrystallized. The thermomechanically affected zone (TMAZ) has been deformed but not fully recrystallized. The heat-affected zone (HAZ) has experienced the thermal cycle without mechanical deformation. The base metal remains unchanged.

The shape and width of these zones depend on tool geometry, rotation speed, travel speed, and cooling. The boundary between the nugget and the TMAZ can be sharp or diffuse. Onion rings seen in an etched cross section are flow marks, not a quality rating. A clean-looking nugget can still contain a void or an incomplete root. A rough-looking surface can have a sound interior. This is why a surface photograph cannot replace a cross section or an agreed NDT check.

Hardness is a practical check. In heat-treatable alloys, the HAZ often shows a local drop in hardness because the thermal cycle alters the precipitate structure. The lowest hardness point may sit outside the nugget. A hardness traverse across the weld, compared with the base metal and the agreed acceptance criteria, tells the reader where the soft zone is and whether the joint is suitable for the load case. A bend test or tensile test adds information about ductility and joint efficiency, but each test answers a different question.

Where the Process Meets Production Reality

Production FSW depends on the fixture as much as the tool. The backing plate supports the workpiece, conducts heat away, and controls the root. A worn or grooved backing plate changes the thermal contact and can leave a mark or a root defect. The clamps must hold the plates flat and prevent them from lifting during plunge. For long panels, the fixture and machine bed must control distortion over the full weld length.

Machine configuration follows the part. A C-type machine is compact and suits small to medium parts, research, and production cells where access around the part matters. A gantry machine carries a larger table and a stiffer bridge for long panels and higher loads. A double-head machine welds two seams in one pass. A 3D machine adds rotary axes for curved surfaces. An extra-length machine handles long straight profiles. The machine is not a generic platform; the table, spindle, force capacity, and control axes must match the joint.

AEE’s C-type FSW machine illustrates how these requirements are packaged for a defined part envelope. The model has a 600 mm by 1200 mm working table, an 8 mm maximum welding thickness, a 30 kN maximum Z-axis force, and a 12 kW spindle with 112 Nm of torque. Those values are product data, not a universal process window. They define the size of part and the force range the machine is built to handle. The tooling, fixture, and procedure still have to be developed for the actual joint.

C-type FSW Machine

For larger panels, the gantry format provides a different tradeoff. The bridge structure carries the welding head over a long table, and the moving mass and stiffness determine how consistently the tool maintains force and position. A gantry machine can be the right choice for battery trays, rail profiles, or ship panels, but the foundation, floor space, and part handling need to be planned before the machine is ordered.

Gantry FSW Machine

Keyhole management is a production decision. A conventional tool leaves a hole at the end of the weld. If the joint is a closed contour or a pressure boundary, that hole may be unacceptable. A retractable tool removes it by withdrawing the pin and filling the cavity. A runoff tab moves it outside the part. For spot joints, refill friction stir spot welding uses a related approach to leave a flat, filled spot.

Retractable FSW Tool

Spot joints follow a related logic: the tool must leave a filled, flat spot rather than an open keyhole. <Refill Friction Stir Spot Welding (RFSSW)> covers refill friction stir spot welding.

How to Check a Weld Visually and What a Photo Cannot Prove

A visual check is useful for screening, not for release. Look at the shoulder mark, the flash, the joint line, the edges, and the start and stop zones. A uniform shoulder mark and controlled flash suggest that the shoulder was in contact and the material was contained. Heavy flash, a dark or rough surface, a visible gap, or a sharp change at the start can point to a parameter or setup problem. Record the location and the parameter trace before adjusting anything.

What you seePossible meaningWhat to do next
Smooth surface with a sharp shoulder markShoulder contact may be excessive or the tool may be diggingCheck plunge depth and tilt against the coupon
Heavy flash along the seamHeat input or axial force may be too highReview rotation speed, force trace, and backing support
Rough or dark surfaceMaterial flow may be unstable or the tool may be wornInspect the tool and compare with a known-good coupon
Visible gap at the joint lineFill may be incomplete or the gap may be too largeStop, check fit-up and clamp pressure, then weld a coupon
Keyhole at the runoutThe exit method may not suit the jointUse a retractable tool, runoff tab, or accept a planned hole

The limits of visual inspection are important. A smooth surface does not prove root consolidation. A filled keyhole does not prove that the nugget is sound. A lack of surface flash does not prove that the axial force was correct. For critical joints, the inspection plan should include a cross section from a representative coupon, an agreed NDT method such as ultrasonic or phased array testing, and mechanical testing where the procedure requires it. The method depends on thickness, joint type, and the acceptance criteria.

A practical first check is to weld a representative coupon with the same tool, fixture, and parameter set, then cut and examine it. Compare the macro section with the agreed standard, check the hardness traverse, and record the result. If the coupon fails, stop the production pass and correct the setup. If the coupon passes, the visual checks on production parts become a screening tool backed by a qualified procedure.

Plan a Coupon Weld for Your Joint

Send the alloy, thickness range, joint type, weld length, and production volume to the FSW engineering team at Aerospace Engineering Equipment (Suzhou) Co., Ltd. The team can review the joint and advise on tooling, machine configuration, and a coupon weld plan. Email [email protected] or call +86 18325808715.

FAQ

Does friction stir welding melt the material?

With FSW, the workpiece stays in the solid state. Heat softens the material and the tool stirs it, but the peak temperature stays below the melting range. This is why FSW avoids solidification porosity and hot cracking in aluminum. The process still needs controlled heat input because too much heat can soften the heat-affected zone, widen the flash, and increase distortion.

Why does FSW leave a keyhole?

A conventional tool leaves a keyhole when the pin withdraws at the end of the pass. The pin has displaced material and the shoulder has contained it, but there is no pin volume left to fill the cavity. A retractable tool or a runoff tab manages the exit. The choice depends on whether the hole sits outside the part, can be removed later, or must be eliminated for a closed contour or pressure boundary.

Can FSW join dissimilar metals?

FSW can join some dissimilar metal pairs, but the window is narrower than for a single alloy. The tool must stir both materials without excessive intermetallic growth, and the interface position and tool offset become part of the procedure. Aluminum to copper and aluminum to steel are active development areas, not drop-in substitutions. A coupon weld and a cross-section check are the first steps before production.

What should I check first when a weld looks smooth but fails inspection?

Start with the cross section and the parameter trace, not the surface. A smooth surface can hide a tunnel, void, or incomplete root. Compare the failed location with the axial force, torque, rotation speed, and travel speed records. Then check the backing plate, clamp pressure, and tool condition. Make one change and verify it on a coupon before revising the production parameter set.

If you’re interested, check out these related articles:

Customized Dissimilar Material Welding Manufacturers in China
Refill Friction Stir Spot Welding (RFSSW)

Let's Build Your Friction Stir Solution

侧边栏